Publish Time: 2023-02-03 Origin: Site
In order to improve the printing efficiency of raw titanium alloy, after internal discussion, the production technology Department decided to use 0.7mm slice thickness to explore and develop the new process, and use the orthogonal experiment scheme of 2 factor ×9 factor (2 supplementary printing samples) , and finally complete the printing. Sandpaper was used to polish the outer shrinkage layer of the sample to a defect free state. The sample density was tested according to the Archimedean drainage method. 99% and relative to 0.5mm layer thickness test density increased. (The Production Technology Department of Guangzhou Sailong/Liang Jingwu)