Views: 0 Author: Site Editor Publish Time: 2022-09-29 Origin: Site
The Logistics Support Department of Guangzhou Sailong continued to study the preparation of 316L film, and made attempts to increase the thickness and resistance of it this week . In terms of increasing the thickness, the method of multiple casting was adopted, and the final film thickness was increased. The thickness of a 2mm plate was only 0.58mm thick at one casting, and the thickness of a 1.2mm plate was 0.83mm thick at three casting.The resistance is increased by adding glass powder, and the effect will be tested in the future.(All members of Logistics Support Department of Guangzhou Sailong)